Lance Hall
New Member
Lance Hall, married to Maureen, StillPoint Pottery
Posts: 17
|
Post by Lance Hall on Feb 23, 2017 11:16:33 GMT -6
Greetings all. has anyone tried using Fusion FZ14 as a sub for Frit 1510 (a European frit manufactured in Netherlands?) I'm interested because I can only get it by ordering a 50 lb. bag from the US (I'm in Canada)so before I spring for a bag I'm wondering if there have been good results using this frit. Thanks in advance for your response.
|
|
bbucky
New Member
Married
Posts: 36
|
Post by bbucky on Feb 23, 2017 16:30:51 GMT -6
I have used it, So far the best tests have been with 3110 combo. 50 to and 50% frit, in moving to 27 % 3110, 25%fz14 with 25,25 on the Zinc and silica next.
|
|
bbucky
New Member
Married
Posts: 36
|
Post by bbucky on Feb 23, 2017 16:57:14 GMT -6
Lance, The firings were to sm cone 11 touching, 2mm thick, and with 1/2 % cobalt carb, and another test with 2% copper carb. Both with 1% titanium and pinches of bentonite. The crystals were deeply refractive and over crowded. Sorrow I haven't been able to post pics, if you text my phone, I'll text some pics back with my notes. 808-989-5143
|
|