gczop
Full Member
Posts: 202
|
Post by gczop on Jun 18, 2016 9:17:59 GMT -6
3110 base adds: 10%frit 3403, 10% Tin Oxide, 1 % Copper carb. Post firing reduction 770c. 3110 base adds: 7% TiO2 2% Antimony Oxide Not Unusual 3110 base adds: 7% TiO2 1% FeOx red. Post firing reduction 770c. 413 base adds 5%FeOx red 2% MnO2 Cheers, G
|
|
Kuba
Full Member
SztukKilka in Old Formu
Posts: 111
|
Post by Kuba on Jun 18, 2016 11:22:05 GMT -6
Did You ever try with bismuth?
|
|
gczop
Full Member
Posts: 202
|
Post by gczop on Jun 18, 2016 12:22:19 GMT -6
Haven't tried bismuth and apart from fuming applications its an unknown to me.
|
|
|
Post by evan cornish-keefe on Jun 19, 2016 23:55:17 GMT -6
Im not familiar with Antimony, what does that do?
I tried a couple little tests with bismuth, other than fluxing the glaze I didn't notice much from it
|
|
|
Post by sherri on Jul 5, 2016 22:24:26 GMT -6
How fun! Thank you for the inspiration!
|
|